The stuff I use is from Lawson...its simular to CopperCoat, but its 80%
copper and works great. it takes very little...*maybe* a tablespoon full to
do a 4 element tribander, but after 4 or 5 years in a really bad salt
environment(Treasure Island in San Francisco bay), everything that had been
put together with this stuff came right apart when the screws were taken
out...anything that didn't get the antiseize was junk.
The stuff is expensive but worth every penny.